Product Parameters:

Tensile strength ≥ 560Mpa

Elongation after break 7%

0.2% specified non-proportional elongation strength Rp0.2: average 590MPa

Young's modulus: average 210GPa

Density: 8.5g/cm3

Coefficient of linear expansion CTE [10-6K-1] 25~500℃ 14. 3

Application: